1.4112 Stainless Steels to BS EN 10088-1

1.4112 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Chemical composition(wt.%) of 1.4112 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.85 0.95
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.015
Cr 17.00 19.00
Ni - -
Mo 0.90 1.30
V 0.07 0.12

1.4112 - Detail

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4112 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
826 (≥) 312 (≥) 43 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade 1.4112 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
877 (≥) 118 (≥) 11 14 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
875 468 716

Equivalent Products