100C6 Air 9160/C Aviation and Aero Steel to AIR 9160 C

100C6 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of 100C6 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.10
Si 0.15 0.35
Mn - 0.35
P - 0.030
S - 0.020
Cr 1.35 1.60
Ni - 0.40
Mo - 0.10
V - 0.30

100C6 Air 9160/C - Detail

100C6 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade 100C6 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
263 (≥) 786 (≥) 13 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade 100C6 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
585 (≥) 928 (≥) 34 12 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
748 173 582

Equivalent Grade

Equivalent Products

We can customize the production of 100C6 Air 9160/C grade, contact us for the best solution.
sales@specificsteel.com