11X13H3 Stainless Steels

11X13H3 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 11X13H3 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.60
Mn - 0.60
P - 0.030
S - 0.025
Cr 12.50 14.50
Ni 2.20 3.00
Mo - 0.30

11X13H3 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 11X13H3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
956 (≥) 193 (≥) 14 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade 11X13H3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
398 (≥) 786 (≥) 42 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
748 142 145

Equivalent Grade

Equivalent Products

We can customize the production of 11X13H3 grade, contact us for the best solution.
sales@specificsteel.com