12Cr18Mn9Ni5N Stainless Steels to GB/T 1220-2007

12Cr18Mn9Ni5N - Specification & Application

  • GB/T 1220-2007 - Stainless steel bars
  • JIS G 4303:1998 -
  • GB/T 1220-1992 - alternate standard

Stainless steel bars

Chemical composition(wt.%) of 12Cr18Mn9Ni5N grade: to GB/T 1220-2007

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.0
Mn 7.5 10.0
P - 0.05
S - 0.03
Cr 17.0 19.0
Ni 4.0 6.0
N 0.05 0.25

12Cr18Mn9Ni5N - Detail

GB/T 1220-2007 standard specifies the stainless steel rods order contents, classification, code, size, shape, weight and allowable deviation, technical requirements, test methods, inspection rules, packaging, logo and certificate of quality.This standard applies to the size is not more than 250 mm hot rolled and forged stainless steel rods.The supply and demand both sides talks things over, can also supply the size larger than 250 mm hot rolled and forged stainless steel rods.

Mechanical properties of grade 12Cr18Mn9Ni5N GB/T 1220-2007

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
658 (≥) 765 (≥) 14 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade 12Cr18Mn9Ni5N GB/T 1220-2007

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
695 (≥) 989 (≥) 24 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
968 695 248

Equivalent Products

We can customize the production of 12Cr18Mn9Ni5N grade, contact us for the best solution.