14Cr-4Mo Stainless Steels to SAE J 467 (1968)

14Cr-4Mo - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

High temperature alloys and other special alloys

Chemical composition(wt.%) of 14Cr-4Mo grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 0.35
Cr - 14.1
Ni - 4.25
Mo - 2.38
Cu - 3.25
Nb - 0.25
N - 0.02
Fe - remaining

14Cr-4Mo - Detail

High temperature alloys and other special alloys

Mechanical properties of grade 14Cr-4Mo SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
745 (≥) 121 (≥) 11 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade 14Cr-4Mo SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
853 (≥) 477 (≥) 22 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
941 661 229

Equivalent Grade

Equivalent Products

We can customize the production of 14Cr-4Mo grade, contact us for the best solution.