15-15 LC Stainless Steels

15-15 LC - Specification & Application

High temperature alloys and other special alloys

Chemical composition(wt.%) of 15-15 LC grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.04
Mn - 15.3
Cr - 16.3
Ni - 1.10
Mo - 1.10
Cu - 0.56
N - 0.40
Fe - remaining

15-15 LC - Detail

High temperature alloys and other special alloys

Mechanical properties of grade 15-15 LC

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
214 (≥) 329 (≥) 33 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade 15-15 LC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
494 (≥) 528 (≥) 42 34 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
222 114 597

Equivalent Grade

Equivalent Products

We can customize the production of 15-15 LC grade, contact us for the best solution.
sales@specificsteel.com