17-14 CuMo Stainless Steels to SAE J 467 (1968)

17-14 CuMo - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of 17-14 CuMo grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.50
Mn - 0.75
P - -
S - -
Ni - 14.10
Cr - 15.90
Al - -
Cu - 3.00
Ti - 0.25
Fe remaining -
Nb - 0.45

17-14 CuMo - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade 17-14 CuMo SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
911 (≥) 959 (≥) 13 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 17-14 CuMo SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
852 (≥) 675 (≥) 43 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
197 354 348

Equivalent Products

We can customize the production of 17-14 CuMo grade, contact us for the best solution.