2357 Stainless Steels to SS 142357

2357 - Specification & Application

  • SS 142357 - Stainless steel - SS steel 2357

Stainless steel - SS steel 2357

Chemical composition(wt.%) of 2357 grade: to SS 142357

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn 7.50 10.00
P - 0.060
S - 0.030
Cr 17.00 19.00
Ni 4.00 6.00
Mo - -
N - 0.25

2357 - Detail

Stainless steel - SS steel 2357

Mechanical properties of grade 2357 SS 142357

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
192 (≥) 233 (≥) 31 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade 2357 SS 142357

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
639 (≥) 482 (≥) 43 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
434 538 781

Equivalent Products

We can customize the production of 2357 grade, contact us for the best solution.