2S.131 Stainless Steels to BS 2S 131

2S.131 - Specification & Application

  • BS 2S 131 - Specification for high thermal expansion steel billets, bars, forgings and parts (620 MPa: limiting ruling section 150 mm)

Specification for high thermal expansion steel billets, bars, forgings and parts (620 MPa: limiting ruling section 150 mm)

Chemical composition(wt.%) of 2S.131 grade: to BS 2S 131

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.55 0.70
Si 0.20 0.50
Mn 3.50 5.50
P - 0.035
S - 0.025
Cr 3.00 4.00
Ni 11.00 14.00
Mo - 0.50
W - 1.00
V - 0.25

2S.131 - Detail

Specification for high thermal expansion steel billets, bars, forgings and parts (620 MPa: limiting ruling section 150 mm)

Mechanical properties of grade 2S.131 BS 2S 131

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
692 (≥) 658 (≥) 44 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade 2S.131 BS 2S 131

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
873 (≥) 871 (≥) 43 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
385 745 886

Equivalent Grade

Equivalent Products

We can customize the production of 2S.131 grade, contact us for the best solution.
sales@specificsteel.com