Chemical composition(wt.%) of 310 grade: to SAE AMS-QQ-S-763B (1998)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - 1.00
Cu - 1.00

310 - Detail

Steel, Corrosion Resistant, Bars, Wire, Shapes, and Forgings

Mechanical properties of grade 310 SAE AMS-QQ-S-763B (1998)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
959 (≥) 175 (≥) 44 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade 310 SAE AMS-QQ-S-763B (1998)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
988 (≥) 877 (≥) 43 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
924 328 182
We can customize the production of 310 grade, contact us for the best solution.