310 Stainless Steels to A 167 (2009)

310 - Specification & Application

  • A 167 (2009) - Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip
  • A 182/A 182M (2012) - Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
  • A 276 (2010) - Stainless Steel Bars and Shapes
  • A 314 (2008) - Stainless Steel Billets and Bars for Forging
  • A 409/A 409M (2008) - Welded Large Diameter Austenitic Steel Pipe for Corrosive or High-Temperature Service
  • A 473 (2009) - Stainless Steel Forgings
  • A 580/A 580M (2012) - Stainless Steel Wire
  • A 632 (2009) - Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service
  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
  • A 965/A 965M (2012) - Steel Forgings, Austenitic, for Pressure and High Temperature Parts
  • SAE AMS-QQ-S-763B (1998) - Steel, Corrosion Resistant, Bars, Wire, Shapes, and Forgings
  • SAE J 467 (1968) - Special Purpose Alloys

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of 310 grade: to A 167 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - 1.00
Cu - 1.00

310 - Detail

Stainless and Heat-Resisting Chromium-Nickel Steel Plate, Sheet, and Strip

Mechanical properties of grade 310 A 167 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
626 (≥) 346 (≥) 14 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade 310 A 167 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
732 (≥) 262 (≥) 32 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
583 669 299
We can customize the production of 310 grade, contact us for the best solution.