314 Stainless Steels to SAE J 467

314 - Specification & Application

  • SAE J 467 - Special purpose alloys (superalloys)

Special purpose alloys (superalloys)

Chemical composition(wt.%) of 314 grade: to SAE J 467

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si 1.50 3.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 23.0 26.0
Ni 19.0 22.0

314 - Detail

Stainless and heat resisting steels

Special purpose alloys (superalloys)

SAE 314

Mechanical properties of grade 314 SAE J 467

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
293 (≥) 369 (≥) 13 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade 314 SAE J 467

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
226 (≥) 999 (≥) 32 31 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
426 156 271