352S52 Stainless Steels to BS 970-4

352S52 - Specification & Application

  • BS 970-4 - Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Chemical composition(wt.%) of 352S52 grade: to BS 970-4

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.45
Mn 8.00 10.00
P - 0.040
S - 0.035
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.38 0.50
C+N 0.90 -
Nb 2.00 3.00

352S52 - Detail

Specification for wrought steels for mechanical and allied engineering purposes. Valve steels

Mechanical properties of grade 352S52 BS 970-4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
286 (≥) 619 (≥) 14 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade 352S52 BS 970-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
755 (≥) 283 (≥) 42 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
285 389 565

Equivalent Grade

Equivalent Products

We can customize the production of 352S52 grade, contact us for the best solution.