422M Stainless Steels to SAE J 467 (1968)

422M - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of 422M grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.85
Si - 0.25
Mn - 0.84
P - -
S - -
Ni - 0.20
Cr - 12.00
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - 2.25
W - 1.70
V - 0.50

422M - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade 422M SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
211 (≥) 963 (≥) 44 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade 422M SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
532 (≥) 969 (≥) 31 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
238 847 588

Equivalent Grade

Equivalent Products