4419 Stainless Steels to A 29/A 29M (2012)

4419 - Specification & Application

  • A 29/A 29M (2012) - Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Chemical composition(wt.%) of 4419 grade: to A 29/A 29M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 0.30
Mn - 1.00
P - -
S - -
Ni - 0.50
Cr - 11.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - 0.50
W - 0.25
V - 0.40

4419 - Detail

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Mechanical properties of grade 4419 A 29/A 29M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
186 (≥) 698 (≥) 12 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade 4419 A 29/A 29M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
188 (≥) 865 (≥) 34 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
679 797 275

Equivalent Products

We can customize the production of 4419 grade, contact us for the best solution.