9Cr-1Mo-V-Cb-N Stainless Steels

9Cr-1Mo-V-Cb-N - Specification & Application

High temperature alloys and other special alloys

Chemical composition(wt.%) of 9Cr-1Mo-V-Cb-N grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.12
Si 0.20 0.50
Mn 0.30 0.60
Cr 8.00 9.50
Ni - 0.40
Mo 0.85 1.05
Al - 0.04
V 0.18 0.25
Nb 0.06 0.10
N 0.03 0.07

9Cr-1Mo-V-Cb-N - Detail

High temperature alloys and other special alloys

Mechanical properties of grade 9Cr-1Mo-V-Cb-N

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
781 (≥) 756 (≥) 42 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 9Cr-1Mo-V-Cb-N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
561 (≥) 188 (≥) 33 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
936 427 377

Equivalent Grade

Equivalent Products

We can customize the production of 9Cr-1Mo-V-Cb-N grade, contact us for the best solution.