A 1031 Grade 8650 Stainless Steels to A 1031/A1031M (2012)

A 1031 Grade 8650 - Specification & Application

  • A 1031/A1031M (2012) - Steel, Sheet and Strip, Heavy-Thickness Coils, Alloy, Drawing Steel and Structural Steel, Hot-Rolled

Steel, Sheet and Strip, Heavy-Thickness Coils, Alloy, Drawing Steel and Structural Steel, Hot-Rolled

Chemical composition(wt.%) of A 1031 Grade 8650 grade: to A 1031/A1031M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 15.00
Cr 17.00 19.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo 1.75 2.75
V - -

A 1031 Grade 8650 - Detail

Steel, Sheet and Strip, Heavy-Thickness Coils, Alloy, Drawing Steel and Structural Steel, Hot-Rolled

Mechanical properties of grade A 1031 Grade 8650 A 1031/A1031M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
852 (≥) 453 (≥) 14 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade A 1031 Grade 8650 A 1031/A1031M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
164 (≥) 391 (≥) 22 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 224
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
253 116 357

Equivalent Products

We can customize the production of A 1031 Grade 8650 grade, contact us for the best solution.
sales@specificsteel.com