Steel, Sheet and Strip, Heavy-Thickness Coils, Alloy, Drawing Steel and Structural Steel, Hot-Rolled
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.03 | ||
Ni | 13.00 | 15.00 | ||
Cr | 17.00 | 19.00 | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
N | - | - | ||
Mo | 1.75 | 2.75 | ||
V | - | - |
Steel, Sheet and Strip, Heavy-Thickness Coils, Alloy, Drawing Steel and Structural Steel, Hot-Rolled
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
249 (≥) | 477 (≥) | 22 | 13 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
186 (≥) | 594 (≥) | 31 | 33 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
462 | 162 | 629 |
We can customize the production of A 1031 Grade 8655 grade, contact us for the best solution.