A 193 347LN Class 1A Stainless Steels to A 193/A 193M (2012)

A 193 347LN Class 1A - Specification & Application

  • A 193/A 193M (2012) - Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications

Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications

Chemical composition(wt.%) of A 193 347LN Class 1A grade: to A 193/A 193M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.005 0.02
Si - 0.75
Mn - 2.00
P - 0.04
S - 0.03
Ni 9.00 13.00
Cr 17.00 20.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.06 0.10
Mo - -
V - -

A 193 347LN Class 1A - Detail

Standard Specification for Alloy-Steel and Stainless Steel Bolting for High Temperature or High Pressure Service and Other Special Purpose Applications

Mechanical properties of grade A 193 347LN Class 1A A 193/A 193M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
346 (≥) 559 (≥) 32 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade A 193 347LN Class 1A A 193/A 193M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
818 (≥) 974 (≥) 21 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
889 814 795

Equivalent Products

We can customize the production of A 193 347LN Class 1A grade, contact us for the best solution.
sales@specificsteel.com