A 213 18Cr-2Mo Stainless Steels to A 213/A 213M (2013)

A 213 18Cr-2Mo - Specification & Application

  • A 213/A 213M (2013) - Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of A 213 18Cr-2Mo grade: to A 213/A 213M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 15.00
Cr 17.00 19.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo 1.75 2.75
V - -

A 213 18Cr-2Mo - Detail

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade A 213 18Cr-2Mo A 213/A 213M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
981 (≥) 533 (≥) 33 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 213 18Cr-2Mo A 213/A 213M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
423 (≥) 481 (≥) 11 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
916 855 297

Equivalent Products

We can customize the production of A 213 18Cr-2Mo grade, contact us for the best solution.