A 268 S43036 Stainless Steels to SA-268/SA-268M

A 268 S43036 - Specification & Application

  • SA-268/SA-268M - Specification for Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Specification for Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Chemical composition(wt.%) of A 268 S43036 grade: to SA-268/SA-268M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 16.00 19.50
Ni - 0.75
Mo - -
Ti 5×C% 0.75

A 268 S43036 - Detail

Specification for Seamless and Welded Ferritic and Martensitic Stainless Steel Tubing for General Service

Mechanical properties of grade A 268 S43036 SA-268/SA-268M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
979 (≥) 766 (≥) 21 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade A 268 S43036 SA-268/SA-268M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
474 (≥) 942 (≥) 43 13 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
389 441 691