A 276 S31100 Stainless Steels to A 276 (2010)

A 276 S31100 - Specification & Application

  • A 276 (2010) - Stainless Steel Bars and Shapes

Stainless Steel Bars and Shapes

Chemical composition(wt.%) of A 276 S31100 grade: to A 276 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn - 1.00
Si - 0.06
P - 0.03
S - 0.03
Cr 25.00 27.00
Ni 6.00 7.00
Mo - -
Ti - 0.25

A 276 S31100 - Detail

Stainless Steel Bars and Shapes

Mechanical properties of grade A 276 S31100 A 276 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
841 (≥) 417 (≥) 12 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade A 276 S31100 A 276 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
728 (≥) 465 (≥) 11 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
674 278 976

Equivalent Grade

Equivalent Products

We can customize the production of A 276 S31100 grade, contact us for the best solution.