Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.08 | 0.15 | ||
Si | - | 0.75 | ||
Mn | 1.00 | 2.00 | ||
P | - | - | ||
S | - | 0.03 | ||
Ni | 8.50 | 10.50 | ||
Cr | 27.00 | 31.00 | ||
Al | - | - | ||
Cu | - | 0.50 | ||
Ti | - | - | ||
Fe | - | - | ||
N | - | - | ||
Mo | - | 0.50 |
Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
252 (≥) | 761 (≥) | 43 | 21 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
639 (≥) | 565 (≥) | 44 | 34 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
154 | 691 | 547 |
We can customize the production of A 29 92L54 grade, contact us for the best solution.