A 29 94B30 Stainless Steels to A 29/A 29M (2012)

A 29 94B30 - Specification & Application

  • A 29/A 29M (2012) - Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Chemical composition(wt.%) of A 29 94B30 grade: to A 29/A 29M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.75
Mn 1.00 2.00
P - -
S - 0.03
Ni 8.50 10.50
Cr 27.00 31.00
Al - -
Cu - 0.50
Ti - -
Fe - -
N - -
Mo - 0.50

A 29 94B30 - Detail

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Mechanical properties of grade A 29 94B30 A 29/A 29M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
714 (≥) 664 (≥) 21 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade A 29 94B30 A 29/A 29M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
433 (≥) 572 (≥) 11 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
228 322 215

Equivalent Products

We can customize the production of A 29 94B30 grade, contact us for the best solution.
sales@specificsteel.com