A 312 S31254 Stainless Steels to A 312/A 312M (2012)

A 312 S31254 - Specification & Application

  • A 312/A 312M (2012) - Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of A 312 S31254 grade: to A 312/A 312M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.020
Si - 0.80
Mn - 1.00
P - 0.03
S - 0.01
Cr 19.5 20.5
Ni 17.5 18.5
Mo 6.00 6.50
Cu 0.50 1.00
N 0.18 0.22

A 312 S31254 - Detail

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Mechanical properties of grade A 312 S31254 A 312/A 312M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
568 (≥) 487 (≥) 33 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade A 312 S31254 A 312/A 312M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
234 (≥) 656 (≥) 34 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
789 225 963

Equivalent Products

We can customize the production of A 312 S31254 grade, contact us for the best solution.