A 312 S32654 Stainless Steels to A 312/A 312M (2012)

A 312 S32654 - Specification & Application

  • A 312/A 312M (2012) - Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of A 312 S32654 grade: to A 312/A 312M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn 2.00 4.00
Si - 0.50
P - 0.03
S - 0.005
Cr 24.00 25.00
Ni 7.00 8.00
Cu 0.30 0.60
N 0.45 0.55

A 312 S32654 - Detail

Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

Mechanical properties of grade A 312 S32654 A 312/A 312M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
925 (≥) 544 (≥) 14 34 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade A 312 S32654 A 312/A 312M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
357 (≥) 763 (≥) 31 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
779 639 473

Equivalent Products

We can customize the production of A 312 S32654 grade, contact us for the best solution.