A 358 S30815 Stainless Steels to A 358/A 358M (2012)

A 358 S30815 - Specification & Application

  • A 358/A 358M (2012) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S30815 grade: to A 358/A 358M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Mn - 0.80
Si 1.40 2.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 10.00 12.00
Mo - -
Al - 1.00
Ce 0.03 0.08

A 358 S30815 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S30815 A 358/A 358M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
476 (≥) 375 (≥) 42 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade A 358 S30815 A 358/A 358M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
282 (≥) 181 (≥) 43 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
314 758 848