A 358 S32654 Stainless Steels to A 358/A 358M (2008)

A 358 S32654 - Specification & Application

  • A 358/A 358M (2008) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S32654 grade: to A 358/A 358M (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn 2.00 4.00
Si - 0.50
P - 0.03
S - 0.005
Cr 24.00 25.00
Ni 7.00 8.00
Cu 0.30 0.60
N 0.45 0.55

A 358 S32654 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S32654 A 358/A 358M (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
648 (≥) 368 (≥) 23 24 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade A 358 S32654 A 358/A 358M (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
455 (≥) 483 (≥) 24 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
811 662 665