A 376 16-8-2H Stainless Steels to A 376/A 376M (2013)

A 376 16-8-2H - Specification & Application

  • A 376/A 376M (2013) - Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service

Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service

Chemical composition(wt.%) of A 376 16-8-2H grade: to A 376/A 376M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.045 0.10
Si - 0.75
Mn - 2.00
Cr 14.5 16.5
Ni 7.5 9.5
Mo 1.50 2.00

A 376 16-8-2H - Detail

Seamless Austenitic Steel Pipe for High-Temperature Central-Station Service

Mechanical properties of grade A 376 16-8-2H A 376/A 376M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
397 (≥) 247 (≥) 11 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 376 16-8-2H A 376/A 376M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
145 (≥) 574 (≥) 34 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
938 395 436

Equivalent Products

We can customize the production of A 376 16-8-2H grade, contact us for the best solution.