A 403 WP 316LN Stainless Steels to A 403/A 403M (2012)

A 403 WP 316LN - Specification & Application

  • A 403/A 403M (2012) - Standard Specification for Wrought Austenitic Stainless Steel Piping Fittings

Intended for pressure piping applications.

Chemical composition(wt.%) of A 403 WP 316LN grade: to A 403/A 403M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

A 403 WP 316LN - Detail

Steel Group: Stainless and heat resisting steels
Subgroup: A 403/A 403M (2012) Standard Specification for Wrought Austenitic Stainless Steel Piping Fittings
Application: Intended for pressure piping applications.

Mechanical properties of grade A 403 WP 316LN A 403/A 403M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
534 (≥) 821 (≥) 42 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade A 403 WP 316LN A 403/A 403M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
523 (≥) 632 (≥) 13 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
997 426 513

Equivalent Products

We can customize the production of A 403 WP 316LN grade, contact us for the best solution.