A 479 N08700 Stainless Steels to A 479/A 479M (2013)

A 479 N08700 - Specification & Application

  • A 479/A 479M (2013) - Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Chemical composition(wt.%) of A 479 N08700 grade: to A 479/A 479M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Mn - 2.00
Si - 1.00
P - 0.04
S - 0.03
Cr 19.00 23.00
Ni 24.00 26.00
Mo 4.30 5.00
Nb 8×C% 0.50
Cu - 0.50
Pb - 0.005

A 479 N08700 - Detail

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Mechanical properties of grade A 479 N08700 A 479/A 479M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
883 (≥) 575 (≥) 12 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade A 479 N08700 A 479/A 479M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
551 (≥) 981 (≥) 13 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
376 585 638

Equivalent Products

We can customize the production of A 479 N08700 grade, contact us for the best solution.