A 493 S44800 Stainless Steels to A 493 (2009)

A 493 S44800 - Specification & Application

  • A 493 (2009) - Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Chemical composition(wt.%) of A 493 S44800 grade: to A 493 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.30
Si - 0.20
P - 0.025
S - 0.02
Cr 28.00 30.00
Ni 2.00 2.50
Mo 3.50 4.20
N - 0.02
Cu - 0.15

A 493 S44800 - Detail

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Mechanical properties of grade A 493 S44800 A 493 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
893 (≥) 913 (≥) 11 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade A 493 S44800 A 493 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
318 (≥) 753 (≥) 12 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
641 676 985