A 580 S31000 Stainless Steels to A 580/A 580M (2012)

A 580 S31000 - Specification & Application

  • A 580/A 580M (2012) - Stainless Steel Wire

Stainless Steel Wire

Chemical composition(wt.%) of A 580 S31000 grade: to A 580/A 580M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.25
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.03
Cr 24.00 26.00
Ni 19.00 22.00
Mo - 1.00
Cu - 1.00

A 580 S31000 - Detail

Stainless Steel Wire

Mechanical properties of grade A 580 S31000 A 580/A 580M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
398 (≥) 759 (≥) 12 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade A 580 S31000 A 580/A 580M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
566 (≥) 945 (≥) 23 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 333
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
133 973 826
We can customize the production of A 580 S31000 grade, contact us for the best solution.