A 580 S44401 Stainless Steels to A 580/A 580M (2012)

A 580 S44401 - Specification & Application

  • A 580/A 580M (2012) - Stainless Steel Wire

Stainless Steel Wire

Chemical composition(wt.%) of A 580 S44401 grade: to A 580/A 580M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Mn - 1.00
Si - -
P - 0.03
S - 0.03
Cr 17.50 19.50
Ni - 1.00
Mo 1.75 2.50
N - 0.035

A 580 S44401 - Detail

Stainless Steel Wire

Mechanical properties of grade A 580 S44401 A 580/A 580M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
515 (≥) 571 (≥) 31 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade A 580 S44401 A 580/A 580M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
283 (≥) 691 (≥) 24 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
659 144 764