A 705 634 Stainless Steels to A 705/A 705M (2009)

A 705 634 - Specification & Application

  • A 705/A 705M (2009) - Age-Hardening Stainless Steel Forgings

Age-Hardening Stainless Steel Forgings

Chemical composition(wt.%) of A 705 634 grade: to A 705/A 705M (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.15
Mn 0.50 1.25
Si - 0.50
P - 0.04
S - 0.03
Cr 15.00 16.00
Ni 4.00 5.00
Mo 2.50 3.25
N 0.07 0.13

A 705 634 - Detail

Age-Hardening Stainless Steel Forgings

Mechanical properties of grade A 705 634 A 705/A 705M (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
377 (≥) 421 (≥) 34 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade A 705 634 A 705/A 705M (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
987 (≥) 882 (≥) 42 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
368 492 852

Equivalent Products

We can customize the production of A 705 634 grade, contact us for the best solution.