A 731 Grade 29-4 Stainless Steels to A 731/A 731M

A 731 Grade 29-4 - Specification & Application

  • A 731/A 731M - Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe

Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe

Chemical composition(wt.%) of A 731 Grade 29-4 grade: to A 731/A 731M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.20
Mn - 0.30
P - -
S - -
Ni - 0.15
Cr 28.00 30.00
Al - -
Cu - 0.15
Ti - -
Fe - -
N - 0.02
Mo 3.50 4.20

A 731 Grade 29-4 - Detail

Seamless, Welded Ferritic, and Martensitic Stainless Steel Pipe

Mechanical properties of grade A 731 Grade 29-4 A 731/A 731M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
932 (≥) 425 (≥) 13 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade A 731 Grade 29-4 A 731/A 731M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
585 (≥) 285 (≥) 42 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
915 138 639

Equivalent Products

We can customize the production of A 731 Grade 29-4 grade, contact us for the best solution.