A 803 Grade 18-2 Stainless Steels to A 803/A 803M (2012)

A 803 Grade 18-2 - Specification & Application

  • A 803/A 803M (2012) - Welded Ferritic Stainless Steel Feedwater Heater Tubes

Welded Ferritic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of A 803 Grade 18-2 grade: to A 803/A 803M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 15.00
Cr 17.00 19.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo 1.75 2.75
V - -

A 803 Grade 18-2 - Detail

Welded Ferritic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade A 803 Grade 18-2 A 803/A 803M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
423 (≥) 816 (≥) 41 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade A 803 Grade 18-2 A 803/A 803M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
243 (≥) 591 (≥) 34 12 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
273 148 191

Equivalent Products

We can customize the production of A 803 Grade 18-2 grade, contact us for the best solution.