A 803 Grade 29-4C Stainless Steels to A 803/A 803M (2012)

A 803 Grade 29-4C - Specification & Application

  • A 803/A 803M (2012) - Welded Ferritic Stainless Steel Feedwater Heater Tubes

Welded Ferritic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of A 803 Grade 29-4C grade: to A 803/A 803M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.20
Mn - 0.30
P - -
S - -
Ni - 0.15
Cr 28.00 30.00
Al - -
Cu - 0.15
Ti - -
Fe - -
N - 0.02
Mo 3.50 4.20

A 803 Grade 29-4C - Detail

Welded Ferritic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade A 803 Grade 29-4C A 803/A 803M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
113 (≥) 229 (≥) 34 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade A 803 Grade 29-4C A 803/A 803M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
852 (≥) 517 (≥) 32 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
418 883 213