A 854 Grade 180 Stainless Steels to A 854/A 854M (2008)

A 854 Grade 180 - Specification & Application

  • A 854/A 854M (2008) - Metallic-Coated Steel Smooth High-Tensile Fence and Trellis Wire

Metallic-Coated Steel Smooth High-Tensile Fence and Trellis Wire

Chemical composition(wt.%) of A 854 Grade 180 grade: to A 854/A 854M (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.50
Mn - 1.00
P - -
S - -
Ni - -
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
W - 3.00

A 854 Grade 180 - Detail

Metallic-Coated Steel Smooth High-Tensile Fence and Trellis Wire

Mechanical properties of grade A 854 Grade 180 A 854/A 854M (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
153 (≥) 497 (≥) 31 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade A 854 Grade 180 A 854/A 854M (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
954 (≥) 484 (≥) 34 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
262 894 138