A 895 S43023 Stainless Steels to A 895 (2009)

A 895 S43023 - Specification & Application

  • A 895 (2009) - Free-Machining Stainless Steel Plate, Sheet, and Strip

Free-Machining Stainless Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of A 895 S43023 grade: to A 895 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Mn - 1.25
Si - 1.00
P - 0.06
S - 0.06
Cr 16.00 18.00
Ni - -
Mo - -
Se - 0.15

A 895 S43023 - Detail

Free-Machining Stainless Steel Plate, Sheet, and Strip

Mechanical properties of grade A 895 S43023 A 895 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
222 (≥) 551 (≥) 31 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade A 895 S43023 A 895 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
966 (≥) 393 (≥) 11 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
475 644 617

Equivalent Products

We can customize the production of A 895 S43023 grade, contact us for the best solution.
sales@specificsteel.com