A 920 Grade 15V41 Class 80 Stainless Steels to A 920/A 920M (2007)

A 920 Grade 15V41 Class 80 - Specification & Application

  • A 920/A 920M (2007) - Steel Bars, Microalloy, Hot-Wrought, Special Quality, Mechanical Properties

Steel Bars, Microalloy, Hot-Wrought, Special Quality, Mechanical Properties

Chemical composition(wt.%) of A 920 Grade 15V41 Class 80 grade: to A 920/A 920M (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.50
Mn - 1.00
P - -
S - -
Ni - -
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
W - 3.00

A 920 Grade 15V41 Class 80 - Detail

Steel Bars, Microalloy, Hot-Wrought, Special Quality, Mechanical Properties

Mechanical properties of grade A 920 Grade 15V41 Class 80 A 920/A 920M (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
537 (≥) 785 (≥) 21 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade A 920 Grade 15V41 Class 80 A 920/A 920M (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
689 (≥) 443 (≥) 14 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
777 995 322