A 965 Grade F316L Stainless Steels to A 965/A 965M (2012)

A 965 Grade F316L - Specification & Application

  • A 965/A 965M (2012) - Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Chemical composition(wt.%) of A 965 Grade F316L grade: to A 965/A 965M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N - 0.10

A 965 Grade F316L - Detail

Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Mechanical properties of grade A 965 Grade F316L A 965/A 965M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
872 (≥) 351 (≥) 13 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade A 965 Grade F316L A 965/A 965M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
141 (≥) 467 (≥) 14 41 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
731 454 639

Equivalent Products

We can customize the production of A 965 Grade F316L grade, contact us for the best solution.