AISI 414 Special Alloy

Chemical composition%of the ladle analysis of gradeAISI 414

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)
0.151.001.000.040.0311.5-13.51.25-2.50
AISI Type 414 is a Martensitic Standard grade Stainless Steel. It is commonly called AISI Type 414 Chromium steel. It is composed of (in weight percentage) 0.15% Carbon (C), 1.00% Manganese (Mn), 1.00% Silicon (Si), 11.5-13.5% Chromium (Cr), 1.25-2.50% Nickel (Ni), 0.04% Phosphorus (P), 0.03% Sulfur (S), and the base metal Iron (Fe). Other designations of AISI Type 414 stainless steel include UNS S41400 and AISI 414.

Steel is the common name for a large family of iron alloys. Steels can either be cast directly to shape, or into ingots which are reheated and hot worked into a wrought shape by forging, extrusion, rolling, or other processes. Wrought steels are the most common engineering material used, and come in a variety of forms with different finishes and properties. Stainless steels are high-alloy steels that have superior corrosion resistance than other steels because they contain large amounts of chromium. Stainless steels contains at least 10% chromium, with or without other elements. Stainless steels can be divided into three basic groups based on their crystalline structure: austenitic, ferritic, and martensitic.
The typical elastic modulus of stainless steels at room temperature (25°C) ranges from 190 to 210 GPa. The typical density of stainless steels ranges from 7.75 to 8.1 g/cm3. The typical tensile strength varies between 515 and 827 MPa. The wide range of ultimate tensile strength is largely due to different heat treatment conditions.

Mechanical properties of gradeAISI 414

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
517(≥) 176(≥) 12 14 42 Solution and Aging,Annealing,Ausaging,Q+T,etc 411

Physical properties of grade AISI 414

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
429(≥) 228(≥) 32 23 42 Solution and Aging,Annealing,Ausaging,Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
363 329 477

AISI 414 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Products