AM-355 Stainless Steels to SAE AMS 5743J (2008)

AM-355 - Specification & Application

  • SAE AMS 5743J (2008) - Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered

Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered

Chemical composition(wt.%) of AM-355 grade: to SAE AMS 5743J (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.40
Mn - 1.00
P - -
S - -
Ni - 4.25
Cr - 15.50
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 2.75
N - 0.10
Co - -

AM-355 - Detail

Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered

Mechanical properties of grade AM-355 SAE AMS 5743J (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
529 (≥) 185 (≥) 34 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade AM-355 SAE AMS 5743J (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
867 (≥) 618 (≥) 32 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
542 784 933

Equivalent Products