B 216 FRTP Stainless Steels to B 216 (2010)

B 216 FRTP - Specification & Application

  • B 216 (2010) - Tough-Pitch Fire-Refined Copper—Refinery Shapes

Tough-Pitch Fire-Refined Copper—Refinery Shapes

Chemical composition(wt.%) of B 216 FRTP grade: to B 216 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 7.50 9.00
P - -
S - -
Ni 5.00 7.00
Cr 17.50 22.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.25 0.50
Mo 2.00 3.00

B 216 FRTP - Detail

Tough-Pitch Fire-Refined Copper—Refinery Shapes

Mechanical properties of grade B 216 FRTP B 216 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
387 (≥) 993 (≥) 24 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade B 216 FRTP B 216 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
922 (≥) 765 (≥) 13 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
832 735 677
We can customize the production of B 216 FRTP grade, contact us for the best solution.