B 622 N12160 Stainless Steels to B 622 (2010)

B 622 N12160 - Specification & Application

  • B 622 (2010) - Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube

Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube

Chemical composition(wt.%) of B 622 N12160 grade: to B 622 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 7.50 9.00
P - -
S - -
Ni 5.00 7.00
Cr 17.50 22.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.25 0.50
Mo 2.00 3.00

B 622 N12160 - Detail

Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube

Mechanical properties of grade B 622 N12160 B 622 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
182 (≥) 911 (≥) 22 11 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade B 622 N12160 B 622 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
426 (≥) 161 (≥) 23 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
616 967 741
We can customize the production of B 622 N12160 grade, contact us for the best solution.