B 739 N08330 Stainless Steels to B 739 (2008)

B 739 N08330 - Specification & Application

  • B 739 (2008) - Nickel-Iron-Chromium-Silicon Alloy Welded Tube

Nickel-Iron-Chromium-Silicon Alloy Welded Tube

Chemical composition(wt.%) of B 739 N08330 grade: to B 739 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 2.00
Si - 1.50
P - 0.045
S - 0.04
Cr 14.00 17.00
Ni 33.00 37.00

B 739 N08330 - Detail

Nickel-Iron-Chromium-Silicon Alloy Welded Tube

Mechanical properties of grade B 739 N08330 B 739 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
598 (≥) 362 (≥) 13 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade B 739 N08330 B 739 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
161 (≥) 145 (≥) 12 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
654 949 378

Equivalent Products

We can customize the production of B 739 N08330 grade, contact us for the best solution.
sales@specificsteel.com