B 783 SS-316L-15 Stainless Steels to B 783 (2010)

B 783 SS-316L-15 - Specification & Application

  • B 783 (2010) - Materials for ferrous powder metallurgy (P/M) structural parts

Materials for ferrous powder metallurgy (P/M) structural parts

Chemical composition(wt.%) of B 783 SS-316L-15 grade: to B 783 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N - 0.10

B 783 SS-316L-15 - Detail

Materials for ferrous powder metallurgy (P/M) structural parts

Mechanical properties of grade B 783 SS-316L-15 B 783 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
744 (≥) 114 (≥) 32 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade B 783 SS-316L-15 B 783 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
343 (≥) 224 (≥) 12 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
468 114 694