B 888 C42200 Stainless Steels to B 888 (2012)

B 888 C42200 - Specification & Application

  • B 888 (2012) - Copper Alloy Strip for Use in Manufacture of Electrical Connectors or Spring Contacts

Copper Alloy Strip for Use in Manufacture of Electrical Connectors or Spring Contacts

Chemical composition(wt.%) of B 888 C42200 grade: to B 888 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.22
Si - 0.40
Mn - 0.75
P - -
S - -
Ni - 0.75
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - 1.00
W - 1.00
V - 0.22

B 888 C42200 - Detail

Copper Alloy Strip for Use in Manufacture of Electrical Connectors or Spring Contacts

Mechanical properties of grade B 888 C42200 B 888 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
764 (≥) 913 (≥) 32 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade B 888 C42200 B 888 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
836 (≥) 479 (≥) 13 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
763 861 668
We can customize the production of B 888 C42200 grade, contact us for the best solution.