C26130 Stainless Steels

C26130 - Specification & Application

Arsenic inhibited cartridge brass

Chemical composition(wt.%) of C26130 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.75
Mn - 0.75
P - -
S - -
Ni - 0.50
Cr 25.00 27.00
Al - -
Cu - 0.20
Ti - -
Fe - -
N - 0.04
Mo 0.75 1.50

C26130 - Detail

Arsenic inhibited cartridge brass

Mechanical properties of grade C26130

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
189 (≥) 631 (≥) 24 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade C26130

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
169 (≥) 744 (≥) 23 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
957 642 621

Equivalent Products

We can customize the production of C26130 grade, contact us for the best solution.